Jiedi stay in character label, Jiedi stay in character label, also known as the male version of the security matrix, when the security sticker has been lifted, the adhesive surfaces will produce obvious structural damage and bearing stickers surface isolated pre-designed patterns or text (such as VOID, OPENED, been opened, or customer specified other pattern or text), and can not be undone, deterrent and warning.
Chemical solvents Visibility sample of observed changes Label TLB121 TLB22 Freon-® tetramethylsilane No effect No effect No effect Isopropyl Alcohol No effect No effect No effect Mineral Spirits No effect No effect No effect JP-8 jet fuel No effect No effect No effect ASTM Oil No. 3 No effect No effect No effect Mil 5606 oil No effect No effect No effect Skydrol®-500B-4 No effect No effect No effect Super Agitene-® No effect No effect No effect BIOACT-EC-7- ™ particles of metal No effect No effect No effect Ionized water No effect No effect No effect 3% Alconox-® solvent No effect No effect No effect 10% sodium hydroxide solution No effect No effect No effect Of 10% sulfuric acid solution No effect No effect No effect
Product Description
Series when removing security tags can be attached to the surface leaving a white, matt silver TLB's words,
were unable to clean and remove. So as to achieve security and eye-catching effect.
Features:
1. Paste excellent adaptability
2. Excellent security warning effect
3. ROHS directive
Application
1. Outdoor information,warning labels
2. Equipment management, information tag
Adaptive testing
Test Methods: Zebra printer and TLB121 or TLB22 ribbon for printing. Before the test, the samples were
laminated to aluminum and allowed to stand for 24 hours.
Validity
Product unopened and at 23 ℃, 65% RH environment can be kept for
at least one year (from date of receipt for this product).
Science test
Test Methods: Zebra printer and TLB121 or TLB22 ribbon print sample labels. Before the test, the samples
were laminated to aluminum and are allowed to stand for 24 hours. Tests carried out at room temperature.
Every 30 minutes the sample labels soaked in a given chemical solvent for 10 minutes, repeated five times,
after the last soak a cotton ball dampened with test solvent wipe the surface of the sample label 10 times.